CR30ni70
Cr30Ni70 (also known as Ni70Cr30) is a high-performance nickel-chromium-based electrical heating alloy. With an optimized chromium (Cr) to nickel (Ni) ratio (30% Cr, 70% Ni), it combines excellent oxidation resistance, high-temperature stability, and uniform resistivity, making it widely applicable in industrial electric Peči, gospodinjski aparati in visokotemperaturna ogrevalna oprema .
Nikelj-kromium električna ogrevalna zlitina CR30ni70 Uvod
Pregled izdelka

Cr30Ni70 (also known as Ni70Cr30) is a high-performance nickel-chromium-based electrical heating alloy. With an optimized chromium (Cr) to nickel (Ni) ratio (30% Cr, 70% Ni), it combines excellent oxidation resistance, high-temperature stability, and uniform resistivity, making it widely applicable in industrial electric Peči, gospodinjski aparati in visokotemperaturna ogrevalna oprema .
Ključne funkcije
Vrhunska visokotemperatura
Najvišja delovna temperatura: 1250 stopinj (dolgoročno stabilno delovanje do 1150 stopinj) .
Oksidacijska odpornost: Visoka vsebnost kroma tvori gosto cr₂o₃ oksidno plast, ki se učinkovito upira visokotemperaturni koroziji .
Stabilne električne lastnosti
Upornost: 1 . 18 μω · m (20 stopinj), z nizko temperaturnim koeficientom za stabilno izhodno moč.
Odpornost toplotne utrujenosti: Stopnja spremembe upora upornosti<2% under thermal cycling.
Odlična mehanska trdnost
Natezna trdnost: Večji ali enak 750 MPa, ohranjanje dobre žilavosti pri visokih temperaturah .
Procesbility: Primerno za risanje žic, valjanje trakov, navijanje in druge kompleksne procese oblikovanja .
Priporočene aplikacije
Natančno industrijsko ogrevanje: Polprevodniške sintranske peči, oprema za vakuumsko toplotno čiščenje .
Gospodinjski aparati: Električne pečice, ogrevalne cevi za kavne stroje .
Ostro okolje: Scenariji, ki zahtevajo pogoste cikle začetka ali ± stopnja natančnosti nadzora temperature .
Izbira navodila
Cr30Ni70 is an upgraded choice over Cr20Ni80 for users prioritizing long lifespan and low maintenance costs with sufficient budget. For ultra-high temperatures (>1300 stopinj), razmislite o kombiniranju s fekralnimi zlitinami .
Priljubljena oznake: CR30NI70, CITAR CR30ni70 Proizvajalci, dobavitelji, tovarna
Primerjava uspešnosti s podobnimi zlitinami
|
Lastnina |
CR30ni70 |
CR20ni80 |
Fecral (0 CR21AL6) |
|
Max Temp |
1250 stopinj |
1200 stopinj |
1400 stopinj |
|
Oksidacijska odpornost |
Odlično (na osnovi CR) |
Dobro |
Zmerno (na osnovi AL, nagnjeni k prašilizaciji) |
|
Upornost (μω · m) |
1.18 |
1.09 |
1.45 |
|
Stroški |
Visok |
Srednje |
Nizka |
|
Prijave |
Natančno ogrevanje |
Splošno ogrevanje |
Ultra visoke peči |