Uvod v Hastelloy

Apr 10, 2025

Hastelloy je zlitina, odporna proti koroziji, ki temelji na nikljevih, v glavnem razdeljena na dve kategoriji: nikelj-kromium zlitina in nikelj-kromium-molibdenska zlitina . Hastelloy ima dobro korozijsko odpornost in toplotno stabilnost in se večinoma uporablja v aviaciji, etchniation, etchy, etcher, etcher, etcher, etchen field, etch
Ameriško podjetje
The company's predecessor, Haynes Stellite Work (Hatz Cobalt-Chromium-Tungsten Factory), was founded in Kokomo, Indiana, USA in 1921. It has a history of 92 years. In the production and research of more than 90 years, it has continuously innovated and invented, thus ranking first in the world in the field of high zlitine .
Haynes International focuses on product production and development. It is mainly engaged in the development and production of high-quality corrosion-resistant and high-temperature resistant nickel-cobalt alloys. The company's expert technicians provide further customer service and technical support worldwide. Haynes' service centers and branches can provide customers with plates, bars, pipes, odkuplje, prirobnice in priključki pravočasno .

You May Also Like